Research article Full text access Get rights and content Gelatin hydrogels loaded with FAKI and ZIF-8@PDA nanoparticles for suppression of hypertrophic scar formation Author links open overlay panelJingjing Su a 1, Mengya Li a 1, Mengbo Xie a, Shengxi Zhou a, Yan Zhang a, Jingan Li b , Kun Zhang a Show more 2026-11-13 科技资讯

Abstract

Hydrogels is an attractive strategy for wound healing. However, it must balance antimicrobial efficacy with biocompatibility, addressing challenges such as insufficient antibacterial properties, limited effectiveness in complex wound healing, and poor scar formation control seen in conventional hydrogel dressings. Herein, we demonstrate an innovative ZIF-8@PDA nanoparticle-embedded gelatin hydrogel with integrated photothermal antibacterial activity (antibacterial rate close to 100% at 3 min) and good biocompatibility. Encapsulation of focal adhesion kinase inhibitors within the hydrogel has an initial release rate of approximately 28% within 24 h in vitro. The combined hydrogels accelerate the closure of bacterially infected inflammatory wounds and reduce the formation of hypertrophic scars in mice. Mechanistically, the hydrogel effectively blocks the mechanotransduction pathway through FAK/ERK/YAP cascade, mitigating fibroblast overproliferation and reducing fibrotic scar formation. These findings highlight a transformative approach in hydrogel design, showcasing the potential to significantly promote wound healing and reduce hypertrophic scar formation, thus paving the way for innovative advancements in next-generation wound management solutions.

Keywords

Hydrogel

;

Hypertrophic scars

;

Polydopamine-coated ZIF-8

1. Introduction

Wound infections can lead to more severe tissue damage and inflammation [1]. It often suffers from excessive repair or even fibrosis, thus leading to hypertrophic scar and keloid [2], [3]. These difficult-to-heal wounds can pose significant risks, placing a significant burden on the physical and mental health of patients and the healthcare system [4]. The dressings such as gauze, foam, sponges and films commonly used in clinic often do not adequately meet the many requirements of the complex wound healing process [5], [6]. Therefore, it is essential to explore a new dressing design with antibacterial and scarless properties for chronic inflammatory wounds.

Hydrogels have been attractive in the biomedical field due to their excellent biocompatibility, adjustable degradability and appropriate mechanical properties [7]. Gelatin has excellent biocompatibility, controllable crosslinking degree and Arginine-glycine-aspartic acid sequence. It can promote platelet aggregation and play a hemostatic effect [8], [9]. In our previous study, gelatin or PCA modified gelatin has reacted with oxidized dextran (Odex) to prepare hydrogels for accelerating wound healing by Schiff base reaction [10], [11]. Zinc-doped hydrogel is a promising bioactive material for wound healing, but it is difficult to control the Zn2+ release [12]. Zeoliticimidazolateframeworks-8 (ZIF-8), as a kind of metal-organic framework [13], is mainly a coordination polymer formed by the cross-linking of N of imidazole or derivatives of imidazole with Zn2+. It is unique in that it has excellent chemical and thermal stability, especially under physiological conditions, sustainable release of Zn2+, while moderate doses of zinc can activate immune regulation and play an active role in angiogenesis and antibacterial processes [14], [15]. Polydopamine (PDA) is widely used in the surface modification of biomaterials because of its good biocompatibility, high photothermal conversion efficiency and self-polymerization properties. Its appropriate photothermal temperature can not only play a bactericidal and anti-inflammatory effect, but also accelerate local blood circulation to promote wound healing [16], [17]. PDA-modified ZIF-8 nanoparticles (ZIF-8@PDA) may combine photothermal activity and sustained antibacterial activity to promote neovascularization and cell proliferation, reduce inflammation, and accelerate wound recovery. For example, a photo crosslinked hydrogel was prepared to kill chondrosarcoma cells and bacteria for the repair of tissue defects after tumor resection [18]. However, while researchers have primarily concentrated on the rate of wound healing, studies aimed at reducing fibrosis and inhibiting scarring remain in their early stages [19]. Therefore, incorporating antifibrotic agents like N-methyl-N-[3-[[[2-[(2-oxo-1,3-dihydroindol-5-yl)amino]-5-(trifluoromethyl)pyrimidin-4-yl]amino]methyl]pyridin-2-yl]methanesulfonamide (PF-562271), a focal adhesion kinase inhibitor (FAKI), into treatment strategies can significantly reduce scar formation. These agents target key pathways involved in fibrosis, thereby minimizing excessive fibroblast activity, collagen deposition, and tissue remodeling that contribute to scarring [20].

Herein, we designed the hydrogel using gelatin, oxidized-dextran, ZIF-8@PDA nanoparticles, and FAKI through Schiff base reaction and physical embedding methods, named GOZPF hydrogel (Fig. 1). Polydopamine-coated ZIF-8 interacts with gelatin via hydrogen bonding and electrostatic interactions, while gelatin crosslinks with oxidized dextran through Schiff base reactions to form the hydrogel network. This hydrogel exhibits excellent photothermal antibacterial properties and scar resistance, alongside a porous three-dimensional network structure. Additionally, the hydrogel's efficacy and mechanisms in promoting skin regeneration were explored at cellular, tissue, and molecular levels. We have therefore demonstrated an ideal wound dressing for advanced wound care and skin regeneration.

Fig. 1
  1. Download: Download high-res image (527KB)
  2. Download: Download full-size image

Fig. 1. Schematic illustration of hydrogels as wound dressings.

2. Materials and methods

2.1. Materials

Gelatin, 3-Hydroxytyramine hydrochloride, Zn(CH3COO)2·2H2O and 2-methylimidazole (2-MI) were bought from Sigma-Aldrich (USA). Dextran was obtained from Solarbio (China). Sodium periodate (NaIO4, Mw 213.89, 98%) were purchased from Aladdin (China). PF-562271 as a model drug of FAKI was bought from MedChemExpress (USA). The polyclonal antibodies including β-actin, goat Anti-Rabbit IgG, TNF-α, IL-6, VEGF and CD31 were obtained from Proteintech Group, Inc. (China). The polyclonal antibodies including α-SMA, MCP-1, YAP/TAZ, P-FAK, FAK, P-ERK and ERK were purchased from CST (USA). The male Kunming mice (30 ± 5 g) were bought from Laboratory Animal Center of Zhengzhou University, and the animals' experiments were approved by the Animal Ethics Committee of Zheng Zhou University.

2.2. Fabrication of the hydrogels

ZIF-8 nanoparticles were prepared by stirring a mixture of Zn(CH3COO)2·2H2O (1 mM) and 2-MI (8 mM) for 20 min at room temperature. Then ZIF-8 nanoparticles (5 mg) were dispersed in 30 mL of Tris-HCl buffer (10 mM, pH 8.5). Subsequently, 3-hydroxytyramine hydrochloride (5 mg) was added dropwise to the suspension under continuous stirring at room temperature. The mixture was allowed to react overnight, followed by centrifugation and washing to isolate the surface-modified ZIF-8@PDA nanoparticles. The preparation of the Odex followed the protocol described previously [10]. Aqueous solutions of Gel (12% w/v) and Odex (2% w/v) were prepared, with the latter containing varying concentrations of ZIF-8@PDA nanoparticles (200, 300, and 400 μg/mL). These solutions were mixed at a 1:1 volume ratio and vigorously homogenized to ensure uniform dispersion. The resulting composite hydrogels were designated as GOZP1, GOZP2, GOZP3 corresponding to the increasing concentrations of ZIF-8@PDA. A control hydrogel containing only Gel and Odex was termed GO. Finally, GOZPF hydrogels were fabricated by incorporating varying concentrations of FAKI (1.25, 2.5, 5, 10, 20 μM) and 300 μg/mL ZIF-8@PDA nanoparticles into the pre-formed aqueous solutions of Gel (12% w/v) and Odex (2% w/v).

2.3. Physical and chemical characterizations

X-ray diffraction spectroscopy (XRD) was used to analyze the crystal structure of ZIF-8 and ZIF-8@PDA nanoparticles. Fourier transform infrared spectrometer (FTIR) was used to detect the functional groups of ZIF-8, ZIF-8@PDA, Dex, Odex, Gel, freeze-dried GO, GOZP and GOZPF hydrogels. The microstructure of nanoparticles and GOZP hydrogel was observed by scanning electron microscope (SEM). The detecting methods of gel formation time, water content, injectable property, self-healing property, rheological property and adhesion property are listed in the supplementary material.

2.4. Photothermal properties

To evaluate the photothermal performance of GOZP hydrogels, samples (100 μL) with varying concentrations were subjected to near-infrared irradiation (NIR, 808 nm, 1.0 W/cm2) for 10 min. Temperature profiles were recorded at 1-min intervals using an infrared thermal camera. GO hydrogels served as controls under identical irradiation conditions. Additionally, the photothermal stability and reversibility of GOZP2 hydrogels (100 μL) were assessed by exposing them to NIR irradiation (808 nm, 1.0 W/cm2) for 5 min, followed by natural cooling for 3 min in the absence of irradiation [21]. The NIR irradiation was cycled 5 times, and the temperature change of hydrogels was recorded by NIR thermography to determine the photothermal stability of hydrogels.

2.5. Antibacterial properties

Liquid dilution antimicrobial assay was adopted in this study. Three experimental groups were set up, namely positive control group (100 μL PBS + 10 μL bacterial suspension), negative control group (100 μL PBS + 10 μL PBS) and experimental group (100 μL hydrogel +10 μL bacterial suspension plus NIR). For the experimental group, 100 μL GOZP2 hydrogel was fabricated in 24-well plates on an ultraclean bench. After hydrogel stabilization, 10 μL diluted bacterial suspension was added dropwise onto the hydrogel, followed by NIR (808 nm, 1 W/cm2) for 0 min, 1 min, 3 min and 5 min, respectively [22]. Subsequently, 1 mL of LB liquid medium was supplemented into each well and incubated for 24 h. The absorbance values of various bacterial suspensions at 600 nm were determined via microplate reader, and the antibacterial inhibition rate was calculated accordingly. In parallel, bacterial suspensions from each group were evenly spread onto agar plates, which were incubated at 37 °C in a constant-temperature incubator for 12 h before colony counting on agar plates was performed.

2.6. Hemocompatibility and histocompatibility

Hemostatic performance and hemolysis assays were conducted with minor modifications based on a previously reported method [11], and the detailed procedures are presented in the supplementary materials. Briefly, nine male Kunming mice were randomly selected and anesthetized with sodium pentobarbital. Subsequently, 100 μL of sterile G hydrogel was slowly injected into the subcutaneous tissue of each mouse using a 1 mL syringe. Three mice were randomly euthanized via perfusion under anesthesia at predetermined time points of 3, 7, and 14 days post-injection. The skin tissues and surrounding muscle at the hydrogel implantation site, as well as major visceral organs including the heart, liver, spleen, lung, and kidney, were harvested. Finally, hematoxylin-eosin (HE) staining was performed to evaluate the inflammatory responses and histological toxicity of the major organs.

2.7. The release of FAKI from GOZPF hydrogels

Three GOZPF hydrogel formulations loaded with varying FAKI concentrations (1.25, 2.5, 5, 10, 20 μM) were fabricated and immersed in small beakers prefilled with 2 mL PBS buffer at 37 °C. At predetermined time points of 12 h, 1, 3, 5 and 7 days, 1 mL of release medium was withdrawn from each beaker, followed by immediate replenishment with an equal volume of prewarmed fresh PBS. Serial FAKI standard solutions with gradient concentrations were subsequently formulated to establish the standard calibration curve of FAKI. Ultimately, the optical density of collected release extracts at each time point was quantified to determine the cumulative drug release profiles.

2.8. Cytocompatibility

Cytocompatibility of GOZP and GOZPF hydrogels was tested by culture of L929 cells and HaCaT cells with hydrogel extract according to the modification of previous reports [10]. The details are provided in the supplementary material.

2.9. Skin scratch healing in vivo

Kunming mice were anesthetized with pentobarbital sodium, removed the hair on the back. Then surgical instruments were used to create a scratch wound with a length of about 10 mm after disinfection. The constructed skin scratch mice were randomly divided into 5 groups with 6 mice in each group, which were Con group, suture group, medical biological glue group, GOZP2 hydrogel group and GOZPF hydrogel group. The wound healing status of mice was photographically recorded on days 0, 3, 6, and 12 post-treatments. On day 12, all mice were anesthetized and euthanized via perfusion. The newly regenerated skin tissues were subsequently harvested for HE and Masson's trichrome staining to assess histological regeneration and tissue remodeling.

2.10. Full- thickness skin wound healing in vivo

A full-thickness circular wound with a diameter of approximately 8 mm was surgically created on the dorsal skin of Kunming mice. Subsequently, 100 μL of Staphylococcus aureus suspension (108 CFU/mL) was inoculated into each wound, and the wounds were maintained for 24 h to establish a stable bacteria-infected wound model. The mice with infected skin wounds were randomly divided into five groups (n = 6 per group): the control (Con) group, Tegaderm film (TM) group, GOZP hydrogel (GOZP) group, GOZP hydrogel combined with NIR irradiation (GOZP+NIR) group, and GOZPF hydrogel combined with NIR irradiation (GOZPF+NIR) group. The Con group received no treatment. The TM group was covered with commercial Tegaderm film (3 M Health Care, USA). The GOZP group was topically administered with 100 μL of GOZP hydrogel. The GOZP+NIR group was treated with 100 μL of GOZP hydrogel followed by 5 min of NIR irradiation (808 nm, 1 W/cm). To distinguish the treatment difference from the GOZP+NIR group, the GOZPF+NIR group received 100 μL of GOZP hydrogel combined with 5 min of NIR irradiation initially, and the GOZP hydrogel was replaced with GOZPF hydrogel starting on day 3 post-treatment. The wound healing progress of mice was photographically monitored on days 0, 3, 7, and 14, and the corresponding wound areas were quantitatively analyzed. On day 14, all mice were anesthetized and euthanized via perfusion. The newly regenerated skin tissues were harvested for HE and Masson's trichrome staining for subsequent histological evaluation.

2.11. Histological staining and Western blot analysis

On the 14th day, the mice were anesthetized and sacrificed by perfusion. Immunofluorescence was used to detect the expression of new tissue related proteins such as Tumor necrosis factor-alpha (TNF-α), Yes-associated protein (YAP), Cluster of differentiation 31 (CD31), Proliferating cell nuclear antigen (PCNA). Immunohistochemistry was used to detect the expression of new tissue related proteins such as α-SMA and matrix metalloproteinases (MMP-9). Western blot was used to detect the expression of related proteins in new tissue. Monocyte chemoattractant protein-1 (MCP- 1), Focal adhesion kinase (FAK), Extracellular signal-regulated kinase (ERK), Yes-associated protein yes/ Transcriptional co-activator with PDZ-binding motif (YAP/TAZ) were selected as important indicators of signal transduction.

2.12. Statistical analysis

GraphPad Prism and Origin were used for plotting, and Two-way ANOVA was used to analyze the experimental results. The data were Mean ± standard deviation (SD), and *P < 0.05 indicated a significant difference, which was statistically significant.

3. Results and discussions

3.1. Characterization of ZIF-8@PDA nanoparticles

The preparation principle of ZIF-8@PDA nanoparticle was shown in Fig. 2A. FTIR analysis of PDA nanoparticles revealed a bending vibration of the indolequinone group at 1507.28 cm−1, confirming the successful synthesis of the PDA nanoparticles. The absorption peak at 1598.77 cm−1 is attributed to the dihydroxyindole and dihydroxyindole carboxylic acid groups, indicating that a Michael addition reaction occurred during the oxidative self-polymerization process of the PDA nanoparticles. FTIR analysis of ZIF-8 nanoparticles revealed bending vibration peaks of the imidazole ring at 693.97, 759.82, 952.99, 1178.68, and 1308.94 cm−1, and stretching vibration peaks of the imidazole ring (Csingle bondN) at 994.51, 1146.6, 1422.48, and 1458.39 cm−1. Moreover, the sharp stretching vibration peak at 421.05 cm−1 (Znsingle bondN) was the characteristic peak of ZIF-8 [23], [24]. FTIR analysis of ZIF-8@PDA nanoparticles revealed peaks at 1576.86 cm−1 (C=N), 1146.08 cm−1 (Csingle bondN), 993.93 cm−1 (Csingle bondN), and 421.31 cm−1 (Znsingle bondN), indicating the successful preparation of the ZIF-8@PDA nanoparticles. (Fig. 2B). The characteristic diffraction peaks at 10.4°, 12.7°, 14.7°, 16.4°, 18.1°, 19.5° and 22.1° correspond to 002, 112, 022, 013, 222, 123 and 114 in the ZIF-8 nano XRD standard PDF card (00–062-1030), respectively, proving that the prepared nanoparticles are ZIF-8 crystals [25]. The XRD peaks of ZIF-8 and ZIF-8@PDA were almost the same, which proved that the crystal structure of ZIF-8 did not change when PDA was wrapped on the surface of ZIF-8, and the crystal structure of ZIF-8 remained intact in ZIF-8@PDA nanoparticles [26] (Fig. 2C). The morphology and size of ZIF-8 and ZIF-8@PDA nanoparticles were observed by SEM (Fig. 2D and E). ZIF-8 was a standard rhomboidal dodecahedron structure [27], their size is around 210 nm, while the ZIF-8@PDA nanoparticles tend to be spherical with slightly larger particle size after wrapping PDA.

Fig. 2
  1. Download: Download high-res image (1MB)
  2. Download: Download full-size image

Fig. 2. Preparation and characterization of ZIF-8@PDA nanoparticles. (A) Schematic diagram of ZIF-8@PDA nanoparticles preparation; (B) FTIR diagram of PDA, ZIF-8, ZIF-8@PDA nanoparticles; (C) XRD diagram of ZIF-8, ZIF-8@PDA nanoparticles; (D) SEM diagram of ZIF-8 and ZIF-8@PDA nanoparticles; (E) TEM diagram of ZIF-8 and ZIF-8@PDA nanoparticles.

3.2. Physicochemical properties of GOZP hydrogels

The amino group on Gel reacts with the aldehyde group on Odex to form GO hydrogel, while ZIF-8@PDA nanoparticles is loaded by physical package to prepare GOZP hydrogel. The existence of an aldehyde stretching vibration peak at 1733 cm−1 indicates the successful synthesis of Odex [1]. The stretching vibration peak of the amino group was found at 3599.08 cm−1 of Gel [28], while the characteristic peaks of the amino group and the aldehyde group were significantly weakened in the GO hydrogel, the GO hydrogel was successfully prepared. The stretching vibration peak of ZIF-8@PDA nanoparticles in GOZP hydrogel indicated that GOZP hydrogel was successfully prepared (Fig. S1A). Gel solution was thoroughly mixed with Odex solution containing ZIF-8@PDA, and the GOZP hydrogel was observed after several minutes (Fig. S1B). The surface of GOZP hydrogel was convex structure, and the inside was loose porous three-dimensional network structure (Fig. S1C). The gelation time of the hydrogels loaded with ZIF-8@PDA nanoparticles was about 4 min (Fig. S1D). The results showed that the water content of the three different concentrations of GOZP hydrogels was above 90% (Fig. S1E), which could provide a moist environment for the wound, reduce the temperature near the wound and relieve the patient's pain, thus facilitating wound healing [29].

The energy storage modulus G' of the three hydrogels with different concentrations was greater than the loss modulus G", and the body phase was more inclined to the characteristics of elastic solid, which proved the formation of stable hydrogels [30], [31]. In addition, the mechanical properties of the hydrogels were improved rapidly after doping with ZIF-8@PDA nanoparticles, because ZIF-8@PDA could interact with hydrogel matrix and increase its stiffness (Fig. S1F).

3.3. Self-healing, injectable properties and adhesive properties of GOZP hydrogels

Injection results showed that GOZP hydrogels could be injected stably and continuously from the needle into water (Fig. S1G). In addition, hydrogels could form different shapes in molds of different shapes (Fig. S1H). GOZP hydrogels with good self-healing properties can effectively solve the problem of hydrogel fracture caused by frequent exercise, thus greatly improving the service life of hydrogel dressings [32]. Macroscopically, the fractured hydrogels were closely bound together and could be stretched to a certain extent (Fig. S1I). The quantitative results of the tensile stresses of the hydrogels showed that the tensile stresses of the spliced and healed hydrogel samples did not change significantly compared with the original hydrogels, which were all around 15 KPa (Fig. S1J).

Currently, wound dressings with excellent adhesion properties can effectively avoid the problem of wound dressing displacement or even dislodgement due to body movements [33], [34]. PDA has strong non-selective adhesion properties to the surface of a wide range of materials [35]. Firstly, GOZP hydrogel was qualitatively tested (Fig. S1K). GOZP hydrogel could adhere the major internal organs of mice cut together well. In addition, it had good adhesion to common materials. To quantify the adhesion properties of GOZP hydrogels, pig skin (simulated human skin) was used as the adhesion substrate material for testing (Fig. S1L). The results indicated that the adhesion strength of hydrogels increased with the increase concentration of ZIF-8 @PDA nanoparticles.

3.4. Photothermal and antimicrobial properties of GOZP hydrogels

PDA modification of ZIF-8 nanoparticles not only reduces their toxicity and enhances their stability, but also imparts photothermal conversion ability to ZIF-8 nanoparticles [36]. After 5 min of NIR irradiation, the GOZP1, GOZP2 and GOZP3 hydrogels warmed up from room temperature of 22 °C to 47.1 °C, 51.3 °C and 61.1 °C, respectively, while the GO hydrogels showed almost no change in temperature under NIR irradiation (Fig. 3A). Numerous studies have shown that when the temperature is around 50 °C, the cell membrane of bacteria will be damaged, causing the denaturation of their proteins and eventually leading to the death of bacteria [37], [38]. The temperature is at a milder state, which does not cause secondary damage to the wound, but also increases the rate of healing of infected wounds by promoting angiogenesis around the wound [39]. Therefore, GOZP2 hydrogels were selected for subsequent experiments. There was no significant difference in the temperature change of GOZP2 hydrogel under five on/off cycles of operation (Fig. 3B). Therefore, GOZP2 hydrogels had good photothermal stability under NIR irradiation.

Fig. 3
  1. Download: Download high-res image (550KB)
  2. Download: Download full-size image

Fig. 3. Photothermal antibacterial properties of hydrogels. (A) Temperature curve and direct view of temperature after 10 min irradiation with GOZP hydrogel NIR (1.0 W /cm2); (B) The temperature change curve of GOZP2 hydrogel under NIR (1.0 W /cm2) on/off cycle irradiation and the direct temperature map of one NIR (1.0 W /cm2) on/off cycle irradiation; (C) Bactericidal rates and images of NIR, GOZP2, GOZP2 + NIR hydrogels against S. aureus and E. coli. (*P < 0.05, n = 3).

Bacterial infection of the wound surface is a major cause of chronic wounds. S. aureus and E. coli are the main pathogens causing wound infections [40]. The results of antibacterial effect of GOZP2 hydrogel with or without NIR are shown in Fig. 3. The antibacterial rate of GOZP2 hydrogel was already close to 100% at 3 min along with the extension of photothermal time, the strains coated on the plates started to decrease or even no colonies were produced. Compared to the Con group, only NIR don't have the antibacterial property, while the GOZP2 group without exposure to NIR also killed a small fraction of bacteria, presumably due to the release of Zn2+ from ZIF-8 degradation.

3.5. Biocompatibility of GOZP hydrogels

3.5.1. Hemocompatibility

The hemolytic property of hydrogels was evaluated by hemolysis test (Fig. S2A and B). The hemolysis rate of GOZP hydrogels was less than 5% as specified by international standards, indicating that the hydrogel was suitable for in vivo treatment [41]. The results showed that the coagulation speed of the hydrogel-treated group was faster than that of the saline-treated group, indicating that the hydrogel in all groups could promote the occurrence of coagulation reaction and accelerate hemostasis (Fig. S2C and D). The hemostatic effect of GOZP hydrogel was evaluated by mouse liver hemorrhage, broken tail hemorrhage and femoral artery hemorrhage models (Fig. S2E、F、G). From the visual images, the bleeding in the GOZP2 hydrogel-treated group was significantly less than that in the control and gauze groups for the three models, indicating that GOZP2 hydrogel could significantly reduce blood loss.

3.5.2. Cytocompatibility and in vivo histocompatibility

To achieve clinical application of hydrogels, the cytocompatibility is critical [42]. The cytotoxicity of different concentrations of hydrogels on HaCaT cells and L929 cells was assessed by cytotoxicity CCK-8 assay. Live/Dead staining of HaCaT and L929 cells revealed negligible cell death after 24 h and 48 h incubation with hydrogel extracts, respectively. Compared with the control group, cells in the hydrogel groups presented uniform distribution and intact morphology (Fig. S3Asingle bondD), confirming the no significantly toxic of GOZP hydrogel toward both cell lines.

The histocompatibility of GOZP2 hydrogel was evaluated by subcutaneous injection in mice. It could be observed that neither the skin nor the muscle in direct contact with GOZP2 hydrogel showed any obvious damage or ulceration, and the hydrogel slowly became smaller with the increase of time, indicating that GOZP2 hydrogel was degraded in mice and no rejection reaction was produced in mice. HE staining was observed to have intact connective tissue, with clearly visible structures such as hair follicles and blood vessels, and no obvious inflammatory cells. Besides, the cells in the hydrogel gradually increased as the time in the body was prolonged, which also reflected the good biocompatibility of the hydrogel. Clear transverse lines of muscle tissue, neat and symmetrical arrangement of muscle fibers, and no obvious inflammatory reaction of muscle tissue were observed, indicating that the hydrogel has good histocompatibility (Fig. S3E). In addition, the degradation products of the hydrogel may be delivered to the whole body of mice through the body circulation, so the main organs of mice were collected for HE staining to further investigate whether GOZP2 hydrogel may cause toxicity to organs [43]. The results showed that the major organs of the GOZP2 hydrogel group were not significantly different from the normal group, inflammatory cells were not significantly detected, and did not cause any significant damage or toxicity, indicating that the hydrogel degradation products were not significantly toxic to the animal organs (Fig. S3F).

The results showed that the survival rate of HaCaT cells and L929 cells gradually decreased with the increase of FAKI concentration (Fig. 4A and 4B). GOZPF hydrogels were synthesized by incorporating FAKI into the GOZP2 hydrogel matrix. FAKI concentration screening and preparation of GOZPF hydrogels can be obtained in Supporting Information (Fig. 4C). FTIR detected the presence of the stretching vibration peak of trifluoromethyl at 1311.4 cm−1 in GOZPF hydrogel, and the results indicated that FAKI was successfully wrapped in GOZP hydrogel (Fig. 4D). The microscopic morphology of GOZPF hydrogel was observed by SEM (Fig. 4E). The inside of GOZPF hydrogel was a porous three-dimensional network structure. The cumulative release amount of FAKI from GOZPF hydrogels gradually increased over incubation time, with an initial drug release rate of approximately 28% within 24 h. Thereafter, the drug release rate gradually decreased. These results demonstrated that the GOZPF hydrogel enabled sustained and prolonged release of FAKI (Fig. 4F). Compared with the results in Fig. 3C, it is shown that adding FAKI will not affect the microstructure of GOZP hydrogel. The results of Live/Dead staining and cell survival rate of HaCaT and L929 cells showed that the proliferation of cells in GOZPF group was less than that in GOZP2 hydrogel group at 24 h, and a small amount of cell death occurred. After 48 h, the number of dead cells in GOZPF group continued to increase, but the cell morphology was not affected. Statistical analysis showed that GOZPF hydrogel could inhibit cell proliferation, thus preventing the problem of scarring caused by the proliferation of fibroblasts (Fig. 4G).

Fig. 4
  1. Download: Download high-res image (732KB)
  2. Download: Download full-size image

Fig. 4. (A) and (B) Changes in the toxicity of different FAKI concentrations on two cell types; (C) Principal diagram of GOZPF hydrogel preparation; (D) FTIR diagram of FAKI, GOZP, GOZPF hydrogel; (E) SEM diagram of GOZPF hydrogel; (F) The release of FAKI from GOZPF hydrogel; (G) AM/PI fluorescence staining and cell survival rate of HaCaT cells and L929 cells incubation with GOZPF hydrogel extracts.

3.6. Inhibitory effect of GOZPF hydrogels on excessive fibrosis in scratch wound healing model

A mouse skin scratch model was used to evaluate the performance of GOZPF hydrogel in acute wound healing (Fig. 5A) [44]. At day 3, both the Con group and the medical bio-glue group showed wound enlargement, and the sutures also appeared to spread. On day 12, the wounds in each group were basically healed, but smaller skin wounds still existed in the con group, and there was obvious scarring after wound closure in both the medical bio-glue and suture groups. Wound closure was complete in the hydrogel group, where the GOZPF hydrogel group had flatter wound closure, while the GOZP2 hydrogel group had the smallest wound closure and the fastest wound healing rate, but there was scar protrusion (Fig. 5B). It is speculated that this may be due to the release of FAKI in GOZPF hydrogel, which slows down the proliferation of fibroblasts near the wound, thus keeping collagen from being over deposited and reducing scar formation.

Fig. 5
  1. Download: Download high-res image (793KB)
  2. Download: Download full-size image

Fig. 5. Evaluation of scratch wound healing in mice. (A) Schematic diagram of skin scratch wound treatment in mice; (B) Visualization of wound healing on days 0, 3, 6, and 12 in mice; (C) HE and Masson staining of new skin tissue from wounds.

A new skin from the healed area was taken for HE and Masson staining after 12 days (Fig. 5C). HE staining showed that the epidermis and subcutaneous tissues in the Con group were not fully formed, with a large number of blood crusts, few neovascularization and a small number of inflammatory cells. In the medical bio-glue group, although the epidermis recovered well, there were still vacancies in its dermis, while in the suture group, the epidermis healed incompletely and the dermis and subcutaneous tissues recovered well, and both wounds were not completely closed. The skin in the GOZPF hydrogel group and GOZP2 hydrogel group recovered well not only from the epidermis but also from the dermis and subcutaneous tissues, and regeneration of skin appendages such as blood vessels, hair follicles and sebaceous glands was significantly increased compared with Con group, medical bio-gel group and suture group. Masson staining results showed that there were more fibroblasts present in the Con group and medical bio-gel group, and the subepidermal new collagen was less and loosely arranged than hydrogel group. A large number of closely arranged fibroblasts and collagen fibers were seen in the suture group, GOZPF hydrogel group and GOZP2 hydrogel group, with a large amount of collagen deposition under the epidermis and abundant granulation tissue. However, the collagen deposition in the GOZPF hydrogel group was more uniform and regular in distribution, similar to normal skin tissue.

3.7. Photothermal antibacterial and anti-excessive fibrosis effect of GOZPF hydrogels in full-thickness skin defect model

The S. aureus infected mouse with full-thickness skin defect model was performed to evaluate the actual effect of GOZPF hydrogel in promoting infected wound healing. The specific operation was shown in Fig. 6A, it should be noted that, for effective antibacterial activity, NIR was applied concurrently with the administration of GOZP2 hydrogel, defined as GOZP2 + NIR. Additionally, half of the samples were subsequently treated with GOZPF hydrogel instead of GOZP2 hydrogel after 3 days, referred to as GOZPF+NIR. The results of the comparison graph of HE staining results showed that the density of inflammatory cells in the infected skin injury was significantly higher than that in the normal skin injury (red arrows), and the results indicated that the infection model of full-thickness skin defect was successfully constructed (Fig. 6B). Fig. 6C showed the wound healing images of mice on days 0, 3, 7 and 14. On day 0, a light-yellow microbial film could be clearly seen covering the wounds of mice, which laterally confirmed the successful construction of the skin infection model. On day 3, it was clearly observed that the wound infection was aggravated in the Con and TM groups, while no aggravation of the infection occurred in the hydrogel photothermal group due to photothermal sterilization. At day 7, the wounds of all groups began to crust. As the treatment time increased, it could be visually seen that the wounds in the hydrogel group were significantly smaller than those in the Con and TM groups, and the wound area of the mice in the GOZP2 + NIR group was the smallest and basically completely healed by day 14, and the same results could be obtained from the wound healing tracings of the mice (Fig. 6D), indicating that the wounds in the GOZP2 + NIR group healed faster. It was observed that the skin of mice in GOZPF+NIR group recovered more smoothly than that in other groups, and there was no hard lump or scar bulge. The GOZP2 hydrogel was replaced with GOZPF hydrogel starting on day 3 post-treatment, showing the early antibacterial phase and better wound healing in the later anti-fibrotic phase. The inhibitory effect of FAKI on cellular activity moderately retarded the rate of wound healing, which was consistent with the reduced cell proliferation observed in the GOZPF group in Fig. 4F. These results indicate that a moderate and appropriate healing rate is essential for favorable wound regeneration. Collectively, these findings indicate that the combined GOZP2 and GOZPF hydrogels is a promising candidate for efficient wound therapy.

Fig. 6
  1. Download: Download high-res image (1MB)
  2. Download: Download full-size image

Fig. 6. Antibacterial effect of infected wound in mice. (A) Schematic diagram of infected wound management with whole cortex injury; (B) HE staining images of infected and non-infected skin wounds on day 0; (C) Tracing images of wound area and wound healing on days 0, 3, 7, and 14; (D) Wound area on days 0, 3, 7, and 14 in each group of mice (* represents P < 0.05 compared with the Con group, n = 6); HE staining (E) and Masson staining (F) of neonatal skin tissue on days 7 and day 14.

Inflammatory cell infiltration (shown by red arrows) was still present in the Con, TM and GOZP2 groups at day 7, although crusting had begun, granulation tissue and epidermis formation was low. The epidermal and subcutaneous tissues in the GOZPF+NIR and GOZP2 + NIR groups recovered well. However, there was a gap between the epidermis and the new granulation tissue in the GOZPF+NIR group, and the epidermal layer was thinner than the other groups (shown in yellow triangle). Angiogenesis is essential for tissue healing and regeneration, and the hydrogel group significantly promoted local angiogenesis (shown by blue arrows in the header). In addition, wound tissue treated with FAKI exhibited significant regeneration of hair follicles, subcutaneous glands (sweat and sebaceous glands) and significant regeneration of subcutaneous adipose tissue (shown by green arrows) (Fig. 6E).

Masson staining is mainly used to evaluate collagen fibrosis in skin tissues. [11] It can dye collagen fibers and mucus blue, cytoplasm and muscle fibers red, and nucleus blue-black. Masson staining results showed that Con group, TM group and GOZP group had less collagen deposition and more muscle fiber formation at day 7. On the contrary, GOZPF+NIR group and GOZP2 + NIR group had more collagen deposition. On the 14th day, it was obviously found that compared with the other four groups, the regenerated skin tissues of the GOZP2 + NIR group showed increased collagen deposition and obvious fibrosis, while the collagen deposition of the GOZPF+NIR group was more orderly, and the structure and shape were closer to normal tissues (Fig. 6F).

3.8. Molecular mechanism

Immunofluorescence and immunohistochemical results of related proteins, and Western blot of newborn skin tissue-associated proteins are shown in Fig. 7. The massive production of neovascularization is crucial for wound healing, and increased positive expression of CD31 indicates an increase in neovascular endothelial cells in the neonatal skin region of mice. The results of immunofluorescence experiments showed a progressive increase of CD31 positive expression. TNF-α is involved in systemic inflammation and can activate neutrophils, endothelial cells, macrophages, and lymphocytes, increasing vascular endothelial cell permeability, and an abnormal increase in TNF-α can lead to excessive inflammation. The results showed that the positive expression of TNF-α was significantly higher in the Con and TM groups than in the other three groups. YAP overexpression may lead to excessive proliferation of fibroblasts to produce large amounts of collagen fibers, which in turn leads to skin scarring [45]. Immunofluorescence results showed that YAP expression was significantly reduced in the GOZPF+NIR group compared to the GOZP2 + NIR group. The experimental results showed that FAKI could inhibit the massive expression of YAP in wounds, thus suppressing the scarring. PCNA positive cells can be used to observe the proliferation of epithelial cells in the epidermal basal cells and skin adnexa of the skin. It was observed that PCNA expression was not continuous in Con group, while PCNA continuity was smoother in the GOZPF+NIR group, suggesting that the GOZPF+NIR group hydrogels promoted the generation of smoother epidermis (Fig. 7A).

Fig. 7
  1. Download: Download high-res image (904KB)
  2. Download: Download full-size image

Fig. 7. Qualitative and quantitative results of wound healing associated proteins. (A) Immunofluorescence images of mouse wound on day 14; (B) Immunohistochemical images of new skin tissue of mouse wound on day 14; The expression (C) and the relative expression (D) of wound protein in each group on day14. (*P < 0.05, n = 3).

As an indicator of mature angiogenesis, α-SMA positive expression was higher in the hydrogel group compared with the Con group, while α-SMA positive expression was slightly lower in the GOZPF+NIR group compared with the GOZP2 + NIR group. Inflammatory factors such as TNF-α released in the early stages of inflammation promote the secretion of MMP-9 by T cells and macrophages, thus allowing a large number of inflammatory cells to reach the trauma surface and further infiltrate into deeper tissues. MMP-9 was selected as an index of inflammatory response in response to the healing process of infected wounds. Compared with the Con and TM groups, MMP-9 was significantly lower in the GOZPF+NIR group, and the expression showed a gradual decrease, which indicated that the GOZPF hydrogel attenuated the wound inflammatory response and could promote orderly wound healing (Fig. 7B).

Different lineages of fibroblasts during wound healing (reticular fibroblasts, myofibroblasts and Papillary fibroblasts, etc.) play a major role, such as reticular fibroblasts secreting the main formation of granulation tissue Collagen fibers, myofibroblasts can shrink wounds and reshape the cellular matrix to promote wound healing [46], [47]. FAK is expressed in keratinocytes, fibroblasts and other skin cells, and is involved in the formation of adhesion between cells and extracellular matrix. Meanwhile, FAK mediates the integrin-involved signaling pathway, which promotes fibroblast proliferation, granulation and angiogenesis, and reduces the production of the inflammatory factor MCP-1 through the FAK- Extracellular signal-regulated kinase (ERK)-YAP/TAZ signaling pathway, thereby accelerating wound healing. However, overexpression of YAP/TAZ leads to excessive proliferation of fibroblasts, causing fibrotic tissue to form at the wound site and leading to scarring. Blocking FAK phosphorylation will inhibit excessive proliferation and migration of fibroblasts and reduce scar production. Phosphorylation of FAK activates ERK, which is essential for endothelial cell migration during revascularization and can promote skin re-epithelialization. The results showed that FAKI significantly prevented the increase of phospho-focal adhesion kinase (p-FAK) levels in the GOZPF+NIR treatment group compared with the GOZP2 + NIR group, resulting in a decrease of phospho-extracellular signal-regulated kinase 1/2 (p-ERK1/2), MCP-1 and YAP/TAZ expression levels (Fig. 7C and D).

These results collectively demonstrate that the engineered hydrogel effectively modulates the wound microenvironment, promotes tissue regeneration, and mitigates hypertrophic scar formation. Specifically, the hydrogel significantly downregulated the expression of pro-inflammatory cytokines (TNF-α, MCP-1), MMP-9, and key components of inflammatory signaling pathways (p-ERK1/2), highlighting its potent anti-inflammatory properties. Concurrently, the upregulation of CD31 suggests enhanced angiogenic activity, which facilitates improved vascularization and accelerates wound healing. Moreover, the reduced expression of α-SMA and YAP/TAZ indicates suppression of myofibroblast activation and fibrotic responses, thereby contributing to the attenuation of pathological scarring.

4. Conclusion

In summary, we demonstrate a hydrogel dressing that exhibits dual therapeutic advantages by effectively combating bacterial infections and significantly suppressing hypertrophic scar formation. In addition to its potent photothermal antibacterial and anti-scarring properties, the GOZPF hydrogel also exhibits a loose and porous three-dimensional network structure, along with excellent injectability, self-healing ability, tissue adhesiveness, hemostatic performance, cytocompatibility, and histocompatibility, making it a highly promising candidate for advanced wound care applications. Mechanistically, the hydrogel promotes wound healing through the upregulation of CD31 expression, thereby enhancing angiogenesis, while simultaneously downregulating pro-inflammatory mediators such as TNF-α, MMP-9, and MCP-1 to attenuate inflammation. Furthermore, the sustained release of FAK inhibitor (FAKI) at later stages suppresses FAK expression, thereby inhibiting the ERK signaling pathway and downregulating YAP expression. This cascade effectively blocks the mechanotransduction pathway, mitigating fibroblast overproliferation and reducing fibrotic scar formation. However, the wound healing process proceeds continuously, and it is difficult to accurately identify the switching time point from the inflammatory phase to the proliferation and remodeling phases. The strategy of replacing hydrogels starting on day 3 in this study is relatively simplistic and arbitrary, which limits the accuracy of the current conclusions. Future studies can focus on developing intelligent systems that can precisely recognize different healing stages and achieve on-demand drug release. In conclusion, this work not only provides a promising strategy for the treatment of infected wounds and scarless skin regeneration but also offers valuable insights for the design and development of next-generation biomaterials for clinical translational applications.

CRediT authorship contribution statement

Jingjing Su: Writing – review & editing, Visualization, Software, Formal analysis, Data curation. Mengya Li: Validation. Mengbo Xie: Methodology, Investigation. Shengxi Zhou: Investigation. Yan Zhang: Validation. Jingan Li: Writing – review & editing, Supervision, Resources, Funding acquisition. Kun Zhang: Writing – review & editing, Supervision, Project administration, Conceptualization.

Declaration of competing interest

The authors declare that they have no known competing financial interests or personal relationships that could have appeared to influence the work reported in this paper.

Acknowledgements

This research was funded by the National Natural Science Foundation of China (Joint Key Projects, U25A20206), and Zhengzhou University Major Project Cultivation Special Project (125-32214076).

Data availability

Data will be made available on request.

References

1

These authors contributed equally to this work.

View Abstract

来源 查看原文

版权申明 本网站立足国家海洋药物和生物制品产业联盟,致力于打造海洋生物医药“产学研用”一站式、综合性资讯共享服务平台,促进我国海洋药物和功能制品“资源链、科技链、产业链、应用链”协同创新、深度融合发展。本文转载自原文来源。版权归原作者及原来出处所有,部分文章未能联系到原作者,在此深表歉意。如涉及版权问题,请留言联系我们协商处理(邮箱:czhang@tio.org.cn),侵权内容将即刻删除。

免责声明 本文仅代表作者个人观点,与本平台立场无关。本站不对内容真实性、完整性、时效性作保证,仅供参考,请读者自行核实。